ABS's appearance is opaque ivory-colored particles, its products can be toned into colorful, and has a 90% high gloss, is widely used in home appliances, automobiles, electronic appliances. ABS material injection molded parts how to increase the brightness of it, the modified plastic editor from the raw material point of view to explain to you.
1、Big differences in particle size of raw materials
Large differences in particle size make it difficult to plasticize uniformly, and bad gloss, for which the raw materials should be sieved and processed.
2, raw material temperature resistance is not good
Some raw materials will be decomposed and discolored at the temperature adjustment, resulting in bad luster, for which the raw materials with better temperature resistance should be used.
3、The additive dispersion is not good
The dispersion of some additives is too poor and makes the plastic parts bad luster, for this, should be replaced with additives with better fluidity.
4、There are too many secondary materials in raw materials
Such as recycled material or water mouth material added too much, affecting the uniform plasticization of the melt and bad luster, which should reduce the amount of recycled material or water mouth material added.
5, the raw materials contain volatile substances
If the moisture or volatile content of raw materials is too high, volatile gas when heated, condensation in the cavity and melt, resulting in poor luster plastic parts, which should be pre-drying raw materials.
6、Impure raw materials
Such as raw materials mixed with foreign materials, miscellaneous materials, or insoluble materials, they can not be mixed with its raw materials evenly melt together and lead to bad luster, which should be strictly excluded beforehand these miscellaneous materials.
7、The amount of lubricant is too little
If the lubricant dosage is too little, the fluidity of the melt is poor, the surface of the plastic part is not dense, which makes the luster bad, for this, the dosage of lubricant should be increased appropriately.
So, also according to your mold polish degree to meet the requirements, if the mold itself is no problem, to determine the characteristics of your ABS to determine, you can choose high mold temperature, high speed, and high pressure; with frozen water can also achieve the degree of finish.
Last: Precision forging and forming technology Next: What is the difference between extruded hollow panels and injection molded hollow panels?
Latest blog posts
Custom molds injection molding
Custom molds injection molding is a manufacturing process that involves creating custom molds to produce plastic parts. Injection molding is a popular technique used in various industries such as...
Plastic injection molding companies
Plastic injection molding is a manufacturing process that involves injecting molten plastic into a mold to create a wide range of plastic products. From car parts to medical devices and household items, plastic injection molding is used to create a variet
PET Preform Injection Moulding Machine
PET preform injection molding is a manufacturing process that is used to create PET (polyethylene terephthalate) preforms that can be later blown into bottles, jars, and other containers. This process...
You may like
13 factors to consider for TPE injection molding process setting
TPE material injection molding prone to problems and solutions!TPE injection molding process refers to the processing of tpe materials to synthesize polymers. Appearance is affected by many factors, in its production...
What is so good about the "all-electric injection molding machine"?
The reason why all-electric injection molding machine is popular in the market is that it has a performance that cannot be achieved by an all-hydraulic injection molding machine, mainly in the following aspects.
Waterproof micro switch low pressure injection molding machine
Waterproof micro switch is a kind of waterproof switch with tiny node build and snap-action structure and external drive lever. Contact spacing is relatively small, also called sensitive switch, snap-action switch. It is a contact structure with a prescri
Four aspects that determine the accuracy of thin-walled injection molded parts
1. Processing of plastic,Because PET macromolecule contains lipid group, has a certain hydrophilic, granules at high temperature is more sensitive to water, when the moisture content...